REFERENCE — TYPES OF CORROSIONDOC CS-REF-04 · REV 1.0

Types of corrosion: 10 forms and how to inspect them

Corrosion is not one thing. The same rust colour can mean slow, even thinning or a crack about to fail. This guide covers the 10 main types of corrosion: what each looks like, where it happens, why, and how it is inspected, including which ones you can see from the surface and which need non-destructive testing (NDT).

01

Why the type of corrosion matters

Different forms of corrosion fail in different ways. Uniform corrosion thins metal slowly and predictably, so you can plan around it. Pitting, cracking and intergranular attack remove very little metal but can cause leaks or sudden fractures. Knowing the type tells you how urgent a finding is and which inspection method can actually measure it.

TypeTypical signFrom the surface?
UniformEven rust, general thinningYes
PittingSmall deep holesExtent yes, depth no
GalvanicAttack at a dissimilar-metal jointYes
CreviceRust bleeding from joints and gapsPartly
FiliformThreads under paintYes
ErosionGrooves along the flowMostly internal
IntergranularLittle visible; grain-boundary attackNo
Stress corrosion crackingFine branching cracksNo
Selective leachingColour change, weak porous metalPartly
MICTubercles, sludge, local pitsLate only
02

Uniform (general) corrosion

VISIBLE FROM THE SURFACE
  • What it looks like: an even layer of rust or tarnish across a wide area, with the metal thinning at a roughly steady rate.
  • Where it happens: exposed carbon steel structures, tanks, roofs, and anything with failed or missing coating.
  • Why it happens: the whole surface is exposed to the same environment, so it corrodes evenly. By tonnage it is the most common form, and the most predictable.
  • How to inspect it: visual survey and area measurement for extent; ultrasonic thickness readings to track wall loss over time.
03

Pitting corrosion

PARTLY VISIBLE
  • What it looks like: small, deep holes, often with a narrow opening and rust or deposits around the edge. The surface can look almost intact while pits go deep.
  • Where it happens: stainless steel and aluminium in chloride environments (seawater, de-icing salt, coastal air), and under deposits on carbon steel.
  • Why it happens: a local break in a protective film becomes a small anode that keeps corroding while the surrounding surface stays passive.
  • How to inspect it: map where pits are and how much area they cover visually; measure pit depth with a pit gauge or ultrasonic testing, because depth, not area, decides the risk.
04

Galvanic corrosion

VISIBLE FROM THE SURFACE
  • What it looks like: accelerated corrosion of one metal right where it touches a different metal, such as a ring of attack around a fastener.
  • Where it happens: steel or aluminium joined to stainless steel or copper, galvanized parts in contact with copper, mixed-metal fasteners and fittings.
  • Why it happens: two different metals in electrical contact, with moisture bridging them, form a battery: the less noble metal corrodes faster. A small anode next to a large cathode is the worst case.
  • How to inspect it: visual inspection at every dissimilar-metal joint; measure the affected area around the contact and recheck it over time.
05

Crevice corrosion

PARTLY VISIBLE
  • What it looks like: attack concentrated in narrow gaps: under gaskets, washers, lap joints, bolt heads and deposits, often with rust bleeding out of the joint.
  • Where it happens: bolted and riveted connections, flanges, lap joints, and anywhere debris sits against the metal.
  • Why it happens: the tiny volume of liquid in the gap runs out of oxygen and becomes more acidic, so the metal inside the crevice corrodes while the outside does not.
  • How to inspect it: look for rust staining and swelling at joints (pack rust can force plates apart); the attack inside the gap usually needs disassembly or NDT to size.
06

Filiform corrosion

VISIBLE FROM THE SURFACE
  • What it looks like: thin, worm-like threads of corrosion creeping under a paint film, starting from a scratch or cut edge.
  • Where it happens: painted or coated aluminium and steel, especially in warm, humid conditions: building cladding, vehicle bodies, window frames.
  • Why it happens: moisture gets under the coating at a defect, and a small corrosion cell travels along under the film, lifting it as it goes.
  • How to inspect it: visual inspection of coated surfaces near edges and damage; measure the affected area to decide between touch-up and recoating.
07

Erosion corrosion

NEEDS NDT TO FIND
  • What it looks like: smooth grooves, gullies or horseshoe-shaped patterns that follow the direction of flow, usually free of corrosion product.
  • Where it happens: pipe elbows and tees, pump impellers, valves, heat exchanger tube inlets, anywhere fluid moves fast or turbulently.
  • Why it happens: moving fluid (often carrying particles or bubbles) strips away the protective layer as fast as it forms, so fresh metal keeps corroding.
  • How to inspect it: mostly internal: ultrasonic thickness surveys at known hotspots, internal visual inspection or borescope when equipment is opened.
08

Intergranular corrosion

NEEDS NDT TO FIND
  • What it looks like: little or nothing on the surface at first; the metal loses strength and can crumble or crack along its grain boundaries.
  • Where it happens: sensitized stainless steel next to welds ("weld decay"), some aluminium alloys, heat-treated components.
  • Why it happens: heat from welding or service changes the chemistry at grain boundaries, making them more reactive than the grains themselves.
  • How to inspect it: laboratory tests, metallography, and NDT such as dye penetrant or eddy current on suspect welds; not something a visual survey can measure.
09

Stress corrosion cracking (SCC)

NEEDS NDT TO FIND
  • What it looks like: fine, branching cracks that can grow with almost no visible corrosion, then lead to sudden failure.
  • Where it happens: austenitic stainless steel in warm chloride environments, carbon steel in caustic or certain pipeline environments, high-strength alloys.
  • Why it happens: it needs three things at once: a susceptible material, tensile stress (applied or left over from welding), and a specific environment.
  • How to inspect it: crack-detection NDT: dye penetrant, magnetic particle, eddy current or ultrasonic methods, targeted at welds and stressed areas.
10

Selective leaching (dealloying)

PARTLY VISIBLE
  • What it looks like: the part keeps its shape but changes colour and becomes weak and porous: brass turns coppery-red (dezincification), cast iron turns soft and graphite-like (graphitic corrosion).
  • Where it happens: brass valves and fittings in water systems, buried or water-carrying cast iron pipe.
  • Why it happens: one element of an alloy (zinc in brass, iron in cast iron) dissolves preferentially, leaving a weak skeleton of the other.
  • How to inspect it: colour change is a visual clue, but the depth of damage needs sectioning, hardness testing or removal for inspection.
11

Microbiologically influenced corrosion (MIC)

NEEDS NDT TO FIND
  • What it looks like: localized pits and tubercles (lumpy deposits) with dark, sometimes smelly sludge underneath; often found where water sits still.
  • Where it happens: water systems, fire sprinkler lines, tank bottoms, pipelines, cooling water, anywhere with stagnant water and deposits.
  • Why it happens: bacteria such as sulfate-reducing bacteria create conditions under deposits that speed up local corrosion.
  • How to inspect it: deposit sampling and microbiological testing, internal inspection and ultrasonic thickness readings; external signs only appear late.
12

Inspecting corrosion by type

A practical survey combines two kinds of method:

  • Surface methods find and size what is visible: uniform rust, galvanic and filiform attack, coating breakdown, the extent of pitting and crevice staining. On coated steel, grade the result with ASTM D610 rust grades.
  • Non-destructive testing finds what is hidden: ultrasonic thickness for wall loss and erosion, dye penetrant, magnetic particle and eddy current for cracks, and specialist methods for corrosion under insulation.

Most structural steel outdoors suffers atmospheric corrosion, which shows up as uniform, pitting, crevice and galvanic attack: the visible types. That is where measuring the affected area each survey pays off.

CorroScan covers the surface part from an iPhone Pro: on-device AI outlines visible corrosion, LiDAR measures its true area in cm² (±6%), and each scan is geotagged so the same areas can be compared from one survey to the next. It does not see inside the metal: depth of pits, cracks and internal corrosion still need NDT.

Visible corrosion is the part you can track every survey. Measure it with CorroScan and see which areas are growing.

FURTHER READING
[1]
AMPP (formerly NACE International) — Forms of corrosion

Industry body for corrosion control; training and reference material on corrosion types.

[2]
M. G. Fontana — Corrosion Engineering

The classic textbook classification of the forms of corrosion.

This page is a general overview in our own words. Diagnosis of a specific failure should be made by a qualified corrosion engineer or inspector.

← Back to CorroScan Atmospheric corrosion → © 2026 OFO Tech · CorroScan® is a registered trademark of OFO Tech
🌐 EN
EnglishEspañolPortuguês (Brasil)DeutschFrançais日本語Bahasa MelayuBahasa IndonesiaไทยTiếng Việt