REFERENCE — ATMOSPHERIC CORROSIONDOC CS-REF-03 · REV 1.0

Atmospheric corrosion on steel structures

Atmospheric corrosion is the rust that forms on steel exposed to air, rain, dew and pollution: the most common kind of corrosion on bridges, towers, plant structures and buildings. This guide covers what drives it, how corrosive a site is, where it starts, and how to inspect and measure it.

01

What atmospheric corrosion is

Steel corrodes in the atmosphere when a thin film of moisture forms on its surface. That film, from rain, dew, fog or high humidity, acts as an electrolyte: iron dissolves at some spots, oxygen is reduced at others, and the products combine into rust. When the surface dries, the reaction stops; when it gets wet again, it starts over.

Because it needs only air and moisture, atmospheric corrosion affects almost every exposed steel asset. It is usually external corrosion: it attacks the outside surface you can see, unlike internal corrosion inside pipes and vessels, buried corrosion in soil, or corrosion hidden under insulation.

02

What drives the corrosion rate

  • Time of wetness: how long the surface stays wet. ISO 9223 counts the hours when relative humidity is above 80% and temperature is above 0 °C. More wet hours, more corrosion.
  • Chlorides: salt from the sea or de-icing salt pulls moisture onto the surface and breaks down protective rust layers. Coastal sites corrode much faster, and the effect falls off with distance from the shore.
  • Sulfur dioxide: from industry and combustion; it acidifies the moisture film and speeds attack.
  • Temperature: warmer, wetter climates, such as humid tropical coasts, combine long wet periods with faster reactions.
  • Deposits and shelter: dirt, bird droppings and debris hold moisture against the steel; sheltered surfaces that never get rinsed by rain can corrode faster than exposed ones.
03

How corrosive is the site? ISO 9223 categories

ISO 9223 sorts environments into six corrosivity categories, measured by how much bare carbon steel corrodes in its first year of exposure. ISO 12944-2 uses the same categories to choose protective paint systems.

CategoryCorrosivitySteel loss, first yearTypical exterior environment
C1Very low≤ 1.3 µmHeated, dry indoor spaces
C2Low1.3 – 25 µmDry or cold climates, rural areas with low pollution
C3Medium25 – 50 µmUrban and light industrial areas; coasts with low salt
C4High50 – 80 µmIndustrial areas; coasts with moderate salt
C5Very high80 – 200 µmAggressive industry with high humidity; coasts with high salt
CXExtreme200 – 700 µmOffshore, splash zones, extreme industrial or tropical marine sites

A first-year loss of 80 µm means a C5 site can eat through a typical paint system's protection quickly once the coating breaks down. That is why the same structure needs a much shorter inspection interval on the coast than inland.

04

Where it starts on steel structures and beams

Atmospheric corrosion rarely starts on a clean, flat, well-drained surface. Look first where water sits or coatings are thin:

  • Edges, corners and welds: paint pulls thin over sharp edges and rough welds, so they rust first.
  • Bolted connections and faying surfaces: crevices between plates trap moisture; rust swelling can force plates apart ("pack rust").
  • Water traps: horizontal flanges, the top of bottom flanges on steel beams, channels facing up, and pockets without drain holes.
  • Bearings, base plates and column feet: where debris collects and water runs down.
  • Below leaking joints and drains: anything regularly wetted by runoff, especially from deck joints on bridges.
  • The sheltered side: undersides and inner faces that collect salt but are never rinsed by rain.
05

How to inspect atmospheric corrosion

  • Plan the survey by zone: split the structure into areas you can name and return to: a span, a girder face, a frame bay.
  • Visual survey: walk each zone, focusing on the hotspots above. Note coating breakdown, rust staining, blistering, flaking and pack rust.
  • Measure the affected area: how much of the surface is rusted, not just whether rust is present. Grade coated surfaces with ASTM D610 rust grades.
  • Check section loss where it matters: where rust is heavy or pitted on load-bearing members, measure remaining thickness with an ultrasonic gauge. Surface measurement shows how much is rusted, not how deep.
  • Photograph and locate every finding: a photo with position and date is what makes next year's inspection comparable.
  • Set the next interval by corrosivity: a C5 coastal site needs a shorter cycle than a C2 inland one.
06

Recording it so the trend shows

One inspection tells you the condition today. The real question is how fast it is changing: which areas are growing, and which asset will need repainting first. That needs the same areas measured the same way each time.

CorroScan turns an iPhone Pro into that measuring tool. On-device AI outlines each corroded region as you aim, LiDAR sizes it in true cm² (±6% area) without a reference marker, and every scan is pinned to GPS with a photo. With the team plan, scans sync to a web console with a live defect map and PDF reports, so growth from one survey to the next is a number, not an impression.

Atmospheric corrosion is slow until it isn't. Measure it every survey with CorroScan and see which areas are growing.

REFERENCES
[1]
ISO 9223 — Corrosion of metals and alloys: Corrosivity of atmospheres, classification, determination and estimation

Corrosivity categories C1–CX, first-year corrosion rates, time of wetness.

[2]
ISO 12944-2 — Paints and varnishes: Corrosion protection of steel structures by protective paint systems, Part 2

Uses the same C1–CX categories to select protective coating systems.

[3]
ASTM D610 — Standard Practice for Evaluating Degree of Rusting on Painted Steel Surfaces

Rust grades 10–0 by percentage of surface rusted. Our explainer and calculator →

This page summarizes the standards in our own words for orientation. For design, specification or contractual use, refer to the current editions from ISO and ASTM.

← Back to CorroScan ASTM D610 rust grades → Types of corrosion → © 2026 OFO Tech · CorroScan® is a registered trademark of OFO Tech
🌐 EN
EnglishEspañolPortuguês (Brasil)DeutschFrançais日本語Bahasa MelayuBahasa IndonesiaไทยTiếng Việt